Pareto — Injection Moulding Defects
A week of cavity-line reject codes typed straight off the check sheet as unquoted labels, computing that 4 of 10 defect modes account for 82.6% of 1,693 rejects and folding the three rarest modes into an explicit Other bar.
Make it your own.
title "Injection moulding rejects — cavity line 2, week 34"
unit rejects
period "Week 34"
threshold 80%
max-bars 8
note "12,480 shots inspected; 100% vision gate on every cavity"
# labels need no quotes when they end in words rather than digits
Short shot 612
Flash 388
Sink marks 241
Weld line 157
Burn marks 96
Warpage 74
Silver streaks 52
Black specks 38
Jetting 21
Flow lines 14